Propiedades
key.properties.Title |
|
---|---|
Density | 0.918 g/cm3 |
Melt Index (g/10min @190°C/2.16 kg (ASTM D1238)) | 1.7 |
typical.properties.Title |
|
---|---|
2% Secant Modulus, MD (ASTM D882) in MPa (psi) | 165 (23900) |
2% Secant Modulus, TD (ASTM D882) in MPa (psi) | 171 (24800) |
Elmendorf Tear Strength, MD (ASTM D1922) in grams (lbs) | 810 |
Elmendorf Tear Strength, TD (ASTM D1922) in grams (lbs) | 1100 |
Gloss (45 degree) | 47 |
Haze (ASTM D1003) | 28.6 % |
Tensile Elongation at Break, MD | 570 % |
Tensile Elongation at Break, TD | 610 % |
Tensile Strength Yield, MD (ASTM D882) in MPa (psi) | 7.74 (1120) |
Tensile Strength Yield, TD (ASTM D882) in MPa (psi) | 8.03 (1160) |