2% Secant Modulus, MD (ASTM D882) in MPa (psi)
|
190 (27600)
|
2% Secant Modulus, TD (ASTM D882) in MPa (psi)
|
175 (25400)
|
Dart Drop Impact (ASTM D1709A) in grams (lbs)
|
120 g (ISO 7765-1a-/A)
|
Elmendorf Tear Strength, MD (ASTM D1922) in grams (lbs)
|
500 g
|
Elmendorf Tear Strength, TD (ASTM D1922) in grams (lbs)
|
400 g
|
Fabrication Method
|
Blown Film Extrusion
|
Functionality
|
Optical Performance, Processing
|
Tensile Elongation at Break, MD
|
450 %
|
Tensile Elongation at Break, TD
|
650 %
|
Tensile Strength Break, MD (ASTM D882) in MPa (psi)
|
17 (2470)
|
Tensile Strength Break, TD (ASTM D882) in MPa (psi)
|
15 (2180)
|
Tensile Strength Yield, MD (ASTM D882) in MPa (psi)
|
9 (1310)
|
Tensile Strength Yield, TD (ASTM D882) in MPa (psi)
|
9 (1310)
|
Vicat Softening Point in °C(°F)
|
93 (199)
|