Propriedades
key.properties.Title |
|
---|---|
Density | 0.939 g/cm3 |
Melt Index ((g/10min @190°C/21.6 kg) (ASTM D1238)) | 22 |
app.properties.Title |
|
---|---|
Anti-block | No |
Slip | No |
typical.properties.Title |
|
---|---|
2% Secant Modulus, MD (ASTM D882) in MPa (psi) | 500 (72500) |
ESCR-Environmental Stress Crack Resistance (10% IGEPAL) | >2000 hr - 50˚C (122˚F) |
Fabrication Method | Pipe Extrusion |
Tensile Elongation at Break, MD | 700 % |
Tensile Strength Break, MD (ASTM D882) in MPa (psi) | 26.0 (3770) |
Tensile Strength Yield, MD (ASTM D882) in MPa (psi) | 20.0 (2900) |
Vicat Softening Point in °C(°F) | 121 (250) |