Properties

key.properties.Title

Density 0.921 g/cm3
Melt Index (g/10min @190°C/2.16 kg (ASTM D1238)) 2

app.properties.Title

Anti-block No
Collation Shrink Usage Retail
Slip No

typical.properties.Title

Dart Drop Impact (ASTM D1709A) in grams (lbs) 96 g
Elmendorf Tear Strength, MD (ASTM D1922) in grams (lbs) 410 g
Elmendorf Tear Strength, TD (ASTM D1922) in grams (lbs) 350 g
Fabrication Method Blown Film Extrusion, Blown Film Extrusion, Cast Film Extrusion, Cast Film Extrusion
Functionality Optical Performance, Processing
Gloss (45 degree) 62
Haze (ASTM D1003) 8 %
Puncture Resistance (Dow Method) in joules/cm3 (lbs/in3) 4 J/cm3 (48.3 ft lb/in3)
Structure Type Monolayer, Multilayer
Tensile Elongation at Break, MD 600 %
Tensile Elongation at Break, TD 830 %
Tensile Strength Break, MD (ASTM D882) in MPa (psi) 23 (3340)
Tensile Strength Break, TD (ASTM D882) in MPa (psi) 19 (2760)
Tensile Strength Yield, MD (ASTM D882) in MPa (psi) 11 (1600)
Tensile Strength Yield, TD (ASTM D882) in MPa (psi) 12 (1740)