Elmendorf Tear Strength, MD (ASTM D1922) in grams (lbs)
|
130 g
|
Elmendorf Tear Strength, TD (ASTM D1922) in grams (lbs)
|
160 g
|
Fabrication Method
|
Blown Film Extrusion, Cast Film Extrusion
|
Functionality
|
Mechanical Performance, Optical Performance
|
Tensile Elongation at Break, MD
|
280 %
|
Tensile Elongation at Break, TD
|
280 %
|
Tensile Strength Break, MD (ASTM D882) in MPa (psi)
|
10 (1450)
|
Tensile Strength Break, TD (ASTM D882) in MPa (psi)
|
7 (1020)
|
Tensile Strength Yield, MD (ASTM D882) in MPa (psi)
|
5 (725)
|
Tensile Strength Yield, TD (ASTM D882) in MPa (psi)
|
4.5 (653)
|